🏆 National e-Governance Award Winner · C4C Industry Platform · 2019
Waterproofing / Site problem guide

Negative-side coating debonding

Internal basement coating blisters while water presses from outside.

A practical decision sequence

Diagnose the cause, then verify the repair.

Use the site evidence to agree a project-specific method with the responsible engineer, concrete producer, manufacturer or specialist applicator.

01 / Symptom

What is happening?

Internal basement coating blisters while water presses from outside.

02 / Inspect and test

Evidence to collect

Measure active seepage and salts; check substrate strength and external drainage options.

03 / Likely mechanism

Why it can fail

Water pressure and salts behind an unsuitable coating can break adhesion.

04 / Technical response

Choose the system

Prefer positive-side treatment where feasible; otherwise design a system rated for negative pressure and treat active paths.

05 / Site execution

Control the application

Remove weak coatings, prepare sound mineral substrate and follow the selected system's moisture limits.

06 / Acceptance

Verify the result

Inspect adhesion and monitor after wet weather or groundwater rise.

Avoid this shortcut

Do not specify a positive-side-only product for reverse pressure.

These guides are editorial starting points, not a project specification. Confirm the design, product data, substrate conditions and inspection plan for the actual site.
Technical references