🏆 National e-Governance Award Winner · C4C Industry Platform · 2019
Admixtures & Concrete / Site problem guide

Excessive entrained air and strength loss

Fresh-air content is high and cylinders show low strength.

A practical decision sequence

Diagnose the cause, then verify the repair.

Use the site evidence to agree a project-specific method with the responsible engineer, concrete producer, manufacturer or specialist applicator.

01 / Symptom

What is happening?

Fresh-air content is high and cylinders show low strength.

02 / Inspect and test

Evidence to collect

Test fresh air and unit weight; review admixture combinations, aggregate and mixing.

03 / Likely mechanism

Why it can fail

Unexpected interaction or dosing can increase air and reduce density.

04 / Technical response

Choose the system

Investigate with supplier and adjust the approved mix only after trials.

05 / Site execution

Control the application

Calibrate dispensers and sample at point of placement.

06 / Acceptance

Verify the result

Trend air, unit weight and compressive strength against project limits.

Avoid this shortcut

Do not infer air content from appearance alone.

These guides are editorial starting points, not a project specification. Confirm the design, product data, substrate conditions and inspection plan for the actual site.
Technical references

References inform the topic; they do not endorse a specific product for this project.

☎